Application of Activated Carbon in Gold Recovery
Dec 30, 2025
Leave a message
In the gold extraction industry, activated carbon is a key material used to adsorb and enrich low-concentration gold from cyanide solutions. Its core function is to selectively enrich gold cyanide complexes in its large pore structure through physical adsorption, achieving a thousand-fold increase in mass concentration and laying the foundation for subsequent efficient recovery.
I. Role of Activated Carbon in Gold Recovery
After cyanide leaching of gold ore, gold exists in the solution as gold cyanide anions (Au(CN)₂⁻) at usually extremely low concentrations. It is economically challenging to directly recover gold from such dilute solutions. Activated carbon, with its extremely high specific surface area (approximately 1000 m²/g) and specific pore structure, becomes an ideal medium for enriching gold from the solution.
In industrial production, coconut shell activated carbon is mainly used. It is produced by steam activation and has sufficient hardness and wear resistance to withstand abrasion in the carbon-in-pulp process.
II. Gold Adsorption Mechanism: Ion Pair Gold cyanide anions are negatively charged, while the surface of activated carbon is electrically neutral, so direct adsorption is not possible. Gold adsorption relies on the formation of "ion pairs". Calcium ions (Ca²⁺, usually from added lime) in the solution combine with two gold cyanide anions to form electrically neutral calcium-gold cyanide ion pairs: Ca[Au(CN)₂]₂. These neutral ion pairs are physically adsorbed on the pore surfaces of activated carbon through van der Waals forces.

This is a reversible dynamic equilibrium process. There is a corresponding relationship between the gold concentration in the solution and the gold load on the activated carbon. To continuously reduce the gold concentration in the solution and increase the gold load on the carbon, a countercurrent contact method is adopted: the gold-bearing pulp flows sequentially through a series of adsorption tanks, while the activated carbon moves in the opposite direction. Fresh carbon is added from the last tank and flows to the first tank with the highest gold concentration; the pulp flows from the first tank to the last tank. In this way, the gold concentration in the tailings discharged from the last tank can be reduced to an extremely low level, while the gold-loaded carbon taken out from the first tank achieves a high load capacity.

III. Main Factors Affecting Gold Adsorption Efficiency Gold adsorption efficiency is affected by various operational and chemical conditions.
1. Physical Conditions: The pulp density needs to be close to the wet density of activated carbon (approximately 1.3-1.5 t/m³) to ensure uniform suspension of carbon particles and avoid sedimentation or floating. Adequate stirring can reduce the thickness of the liquid boundary layer on the surface of carbon particles and accelerate the mass transfer and diffusion of gold into the carbon particles.
2. Activated Carbon Properties: Smaller carbon particle size is beneficial to accelerating adsorption kinetics but increases the difficulty of screening and recovery. Industrially, the commonly used particle size range is 1-3 millimeters (e.g., 6×12 mesh or 8×16 mesh). The hardness of carbon is crucial, as it needs to withstand abrasion during stirring, pumping, and regeneration processes. Coconut shell carbon performs excellently in this regard.
3. Competitive Adsorption and Poisons: This is a key issue affecting recovery rate.
- Organic Poisons: Organic substances such as flotation reagents (e.g., xanthates), lubricating oils, and humic acids compete with gold for adsorption sites and may even block pores. Certain flotation reagents can reduce the adsorption activity of activated carbon by more than 60%. These organic poisons are mainly removed through subsequent thermal regeneration steps.
- Inorganic Poisons: Mainly cyanide complexes of other metals (e.g., copper, nickel, silver). They can also form ion pairs to be adsorbed, occupying active sites. Special attention should be paid to the impact of copper. Its cyanide form in the solution changes with pH, and it is more easily adsorbed when the pH is below 10.5. Most inorganic poisons can be removed by acid washing.
- Scaling: During the CIP process, calcium ions and carbonate may form precipitates such as calcium carbonate (CaCO₃) on the surface of activated carbon. These scale layers are mainly deposited and block the entrances of mesopores and macropores of carbon particles, hindering the diffusion of gold into micropores. Regular acid washing can effectively remove these scale layers.
4. Solution Chemical Environment:
- pH and Cyanide Concentration: Industrially, the pH is usually maintained between 10-11 to control the generation of toxic HCN gas. Sufficient free cyanide concentration is a necessary condition to ensure the effective dissolution and stability of gold.
- Temperature: Gold adsorption is an exothermic process, so lower temperatures are conducive to adsorption. Many factories often achieve higher recovery rates in cold seasons. In contrast, the subsequent desorption process requires high temperatures.
- Ionic Strength: The presence of alkaline earth metal ions such as calcium and magnesium is necessary for the formation of gold cyanide ion pairs.
IV. Desorption: Desorbing Gold from Activated Carbon The gold-loaded carbon adsorbed with high-concentration gold needs to undergo desorption (elution) treatment to transfer gold back to the solution for electrolytic purification.
The basic principle of desorption is to create conditions unfavorable for adsorption and reverse the adsorption process. Industrially, two mature processes are mainly adopted: the AARL method and the Zadra method. Both are based on the following steps:
1. At high temperature, a high-concentration sodium ion (from sodium hydroxide) solution is used to replace calcium ions in the gold cyanide ion pairs with sodium ions through ion exchange, forming less stable sodium-gold cyanide ion pairs.
2. High temperature promotes the decomposition of unstable sodium-gold cyanide ion pairs, and gold cyanide anions are released back into the solution from the surface of activated carbon.


The main difference between the two lies in the process combination: the AARL method is a batch operation, and the desorbed gold-rich solution (pregnant solution) is sent to an independent electrolysis workshop; the Zadra method connects the desorption column and electrolytic cell in series to form a closed-loop cycle, realizing desorption and electrolysis simultaneously. Regardless of the method adopted, the goal is to reduce the gold content of the lean carbon returned to the adsorption circuit to below approximately 50 grams per ton to restore its adsorption capacity.
V. Main Process Flows: CIP, CIL, and Pumpcell
There are three main forms of activated carbon gold extraction processes:
Carbon in Pulp (CIP): The ore first completes most of the gold dissolution through independent cyanide leaching tanks, and then the pulp enters a series of adsorption tanks for gold adsorption. The pulp flows forward, and the activated carbon is transported countercurrently. Its "enrichment ratio" (ratio of gold-loaded carbon grade to feed solution gold grade) is usually 1000-1200.

Carbon in Leach (CIL): Leaching and adsorption are combined and carried out simultaneously in the same series of tanks. This process is particularly suitable for ores containing "gold-robbing" substances (other substances that can adsorb gold), because activated carbon can compete with them to protect the dissolved gold. However, due to the low gold concentration in the solution when leaching is incomplete, a larger inventory of activated carbon is usually required, and the enrichment ratio is generally 800-1000.

Pumpcell Process: Adopts an operation mode similar to a "merry-go-round". Countercurrent flow is achieved by regularly rotating the pulp feed point and tailings discharge point without the need for physical movement of carbon pulp. This method reduces backmixing, manages carbon in batches, can achieve a higher enrichment ratio (1500-2500 or higher), and has a more compact equipment volume.

The process selection depends on various factors such as ore properties, design scale, investment, and operating costs.
VI. Process Monitoring and Balance The stable operation of a CIP/CIL plant relies on the monitoring of key parameters, which is mainly evaluated through two "aspects":
- Gold Concentration in Solution: Monitor the gold content in the solution at the outlet of each adsorption tank, which should show a significant step-by-step downward trend.
- Gold Concentration in Gold-loaded Carbon: Monitor the gold load of activated carbon in each adsorption tank, which should show a step-by-step downward trend from front to back.
Regular analysis of these aspects, combined with tests on the adsorption kinetic rate (activity) of activated carbon, can help the plant timely identify problems such as poison accumulation, reduced equipment efficiency, or operational imbalance, thereby maintaining the optimal gold recovery rate.
Activated carbon plays an irreplaceable role in gold recovery. From the basic principle of adsorbing gold cyanide ion pairs, to addressing the practical challenges of organic and inorganic poisons and scaling, to desorption recovery and process selection, the entire process constitutes a complex and efficient technical system. In-depth understanding and precise control of activated carbon properties, process conditions, and system balance are the core of achieving efficient and economical gold recovery.